History and development of TM0284, Corrosion 1999, NACE Conf. Series, paper n°422, 1999. ,
Conditions of hydrogen-induced corrosion occurrence of X65 grade line pipe steels in sour environments, vol.60, pp.1113-1121, 2004. ,
, NACE committee report 8X294: review of published litterature on wet H2S cracking, 1999.
Overview of hydrogen induced cracking (HIC) of pressure vessels in upstream operations, Corrosion 1991, NACE Conf. Series, paper n°10, 1991. ,
Hydrogen-induced damage in sour, wet crude pipelines, Journal of Petroleum Technology, pp.613-618, 1984. ,
Corrosion of carbon steel by H2S in CO2 containing oilfield environments, Corrosion 2006, NACE Conf. Series, paper n°115, 2006. ,
An overview of european federation of corrosion documents EFC16 and EFC17, Corrosion 1999, NACE Conf. Series, paper n°423, 1999. ,
Fit-for-purpose HIC assessment of large diameter pipes for sour service application, Corrosion 2006, NACE Conf. Series, paper n°124, 2006. ,
Influence of material properties and laboratory test conditions on SOHIC at line pipe carbon steels, Corrosion 1998, NACE Conf. Series, paper n°260, 1998. ,
The condition of HIC occurence of X65 linepipe in wet H2S environments, Corrosion 1999, NACE Conf. Series, paper n°429, 1999. ,
HIC assessment of low alloy steel line pipe for sour service application -Literature survey, 3R International, vol.44, pp.409-417, 2005. ,
Hydrogen induced cracking (HIC) -Laboratory testing assessment of low alloy steel linepipe, Corrosion 2008, NACE Conf. Series, paper n°110, 2008. ,
, Hydrogen-Induced Cracking of Linepipe Steels .1. Threshold Hydrogen Concentration and pH, vol.49, pp.17-23, 1993.
Hydrogeninduced cracking of line pipe steels used in sour service, Corrosion, vol.49, issue.7, pp.531-535, 1993. ,
A study of internal hydrogen embrittlement of steels, Materials Science and Engineering A-Structural Materials Properties Microstructure and Processing, vol.286, issue.2, pp.269-281, 2000. ,
Prediction of sulfide stress cracking in high-strength tubulars, Corrosion, vol.50, issue.7, pp.537-545, 1994. ,
Effect of line pipe steel microstructure on susceptibility to sulfide stress cracking, Corrosion, vol.60, issue.3, pp.244-253, 2004. ,
SSC resistance of a 125 KSI steel grade in slightly sour environments, Corrosion 2005, NACE Conf. Series, paper n°88, 2005. ,
Effect of Molybdenum on Sulfide Stress Cracking Resistance of Low-Alloy Steels, Corrosion, vol.50, issue.9, pp.695-704, 1994. ,
Comparing hydrogen permeation rates, corrosion rates and sulphide stress cracking resistance for C-110 and P-110 casing steel, Corrosion 2007, NACE Conf. Series, paper n°109, 2007. ,
Application of hydrogen permeation for monitoring sulfide stress cracking susceptibility, Corrosion 2002, NACE Conf. Series, paper n°342, 2002. ,
Sulfide stress cracking and corrosion fatigue of steels dedicated to bottom hole assembly components, Corrosion 2005, NACE Conf. Series, paper n°85, 2005. ,
Sulfide stress cracking of a pipeline weld in sour gas service, Corrosion 1999, NACE Conf. Series, paper n°428, 1999. ,
Sulfide stress corrosion cracking and fatigue crack growth of welded TMCP API 5L X65 pipe-line steel, International Journal of Fatigue, vol.23, issue.2, pp.103-113, 2001. ,
Hydrogen permeation studied by electrochemical techniques, Electrochimica Acta, vol.44, issue.24, pp.4431-4442, 1999. ,
Hydrogen diffusion in alphairon studied using an electrochemical permeation transfer function, Electrochimica Acta, vol.44, issue.16, pp.2693-2704, 1999. ,
The use of a permeation technique to predict critical concentration of H 2 for cracking, Corrosion Science, vol.27, pp.1169-1181, 1987. ,
The mechanism of hydrogen evolution on iron in acid solutions by determination of permeation rates, Journal of the Electrochemical Society, vol.111, issue.5, pp.619-623, 1964. ,
Transfer function analysis of hydrogen permeation through a metallic membrane in a Devanathan cell -Part II: Experimental investigation on iron membrane, Journal of Electroanalytical Chemistry, vol.590, issue.1, pp.15-25, 2006. ,
Effect of environmental factors on hydrogen permeation in line pipe steel, vol.44, pp.738-744, 1988. ,
Correlation between critical hydrogen concentration and hydrogen damage of pipeline steel, International Journal of Hydrogen Energy, vol.22, pp.279-284, 1997. ,
Effect of steel microstructure on hydrogen permeation behavior and the determination of critical hydrogen flux for hydrogen embrittlement, Corrosion 2006, NACE Conf. Series, paper n°438, 2006. ,
The relationship between hydrogen permeation and sulfide stress cracking susceptibility of OCTG materials at different temperatures and pH values, Corrosion 1997, NACE Conf. Series, paper n°47, 1997. ,
Hydrogen permeation through ARMCO iron membranes in sour media, Corrosion 2004, NACE Conf. Series, paper n°740, 2004. ,
Effect of alloying elements on the susceptibility to sulfide stress cracking of line pipe steels, Corrosion, vol.60, issue.3, pp.262-274, 2004. ,
Hydrogen permeation in a low carbon martensitic stainless steel exposed to H2S containing brines at free corrosion, Corrosion 1999, NACE Conf. Series, paper n°609, 1999. ,
hydrogen permeation in supermartensitic stainless steels dependent on heat treatment and chemical composition, Corrosion 2000, NACE Conf. Series, paper n°141, 2000. ,
Permeation measurments on thin steel membranes, Corrosion 2002, NACE Conf. Series, paper n°36, 2002. ,
Ultrasensitive technique for detection of hydrogen emanating from steel and other solid surfaces, Materials Science and Technology, vol.16, pp.41-46, 2000. ,
hydrogen flux and high temperature acid corrosion, Corrosion 2006, NACE Conf. Series, paper n°436, 2006. ,
Examples of use and interpretation of field data using a portable hydrogen permeation monitor, NACE Conf. Series, p.477, 2004. ,
Hydrogen permeation flux data correlation with inline corrosion monitoring techniques mapped over location and time, NACE Conf. Series, paper n°636, 2001. ,
Filed application of a new, portable, non-intrusive hydrogen monitor for sour service, Corrosion 2000, NACE Conf. Series, paper n°471, 2000. ,
A laboratory study of types of corrosion inducing hydrogen permeation through steel, Corrosion 2004, NACE Conf. Series, paper n°472, 2004. ,
Measurement of hydrogen permeation through structural steel sections of varying thickness at 19 degrees C, Materials Science and Technology, vol.21, issue.3, pp.347-351, 2005. ,
Practical applications of hydrogen permeation monitoring, Corrosion 2004, NACE Conf. Series, paper n°476, 2004. ,
The hydrogen evolution kinetics and hydrogen entry into a-iron, Journal of the Electrochemical Society, vol.112, issue.10, pp.1025-1031, 1965. ,
Analysis of hydrogen evolution and entry into metals for the discharge-recombination process, Journal of the Electrochemical Society, vol.136, issue.9, pp.2463-2470, 1989. ,
Hydrogen sulfide effect on hydrogen entry into iron -A mechanistic study, vol.46, pp.460-468, 1990. ,
Corrosion Mechanisms in Theory and in Practice, chapter n°3, vol.2, pp.53-96, 2002. ,
, Standard practice for evaluation of hydrogen uptake, permeation, and transport in metals by an electrochemical technique, ASTM G148-97 (revised 2003)
The mathematics of diffusion, 1975. ,
Construction of a universal scale of severity for hydrogen cracking, Corrosion 2000, NACE Conf. Series, paper n°127, 2000. ,
Revisiting hydrogen in steel, part I: theoretical aspects of charging, stress cracking and permeation, NACE Conf. Series, paper n°67, 2001. ,
Revisiting hydrogen in steel, part II: experimental verifications, Corrosion 2001, NACE Conf. Series, paper n°72, 2001. ,
Guidelines on materials requirements for carbon and low alloy steels for H 2 S-containing environments in Oil and Gas production, The Institute of Materials, 1995. ,
A thin palladium coating on iron for hydrogen permeation studies, Electrochimica Acta, vol.41, issue.3, pp.359-365, 1996. ,
The electrochemical permeation of hydrogen in steels without palladium coating. Part I: Interpretation difficulties, Corrosion Science, vol.37, issue.11, pp.1773-1783, 1995. ,
Necessity of a palladium coating to ensure hydrogen oxidation during electrochemical permeation measurements on iron, Electrochimica Acta, vol.40, issue.7, pp.867-871, 1995. ,
Electrochemical study of carbon steel corrosion in buffered acetic acid solutions with chlorides and H 2 S, Electrochimica Acta, vol.48, issue.2, pp.135-144, 2002. ,
Hydrogen permeation through mild steel in temperature range 20-500°C measured by hydrogen collection method, Materials Science and Technology, vol.18, issue.8, pp.851-855, 2002. ,
, Predicting CO 2 corrosion in the oil & gas industry, The Institute of Materials, 1994.